Encapsulated O Ring adopts special rubber resisting high temperature, F+ plastic and special engineering to compound this sealing product. It not only has low contraction permanent set functions of rubber O Ring, but also resistant heat, cold oil, friction, chemical corrusion and other performances. It can be used in all kind of dynamical seal and static seal widely, meanwhile can replace all traditional rubber and plastic O Ring.
Technical Data Sheet
|
Property |
Unit |
Result |
|||
|
A |
B |
C |
|||
|
Normal Conditions |
Hardness |
JIS Hs |
70~90 |
70~90 |
60~75 |
|
Elongations(min.) |
% |
60 |
60 |
80 |
|
|
Tensile Stress(min) |
Mpa |
16 |
16 |
16 |
|
|
Compressibility |
% |
50~60 |
50~60 |
60~75 |
|
|
Recovery |
% |
>85 |
>85 |
>70 |
|
|
Permanentset |
% |
<10 |
<10 |
<10 |
|
|
230°Cx24h hot air ageing |
Change of hardness(max) |
JIS Hs |
-5~+5 |
-5~+5 |
-5~+5 |
|
Change of Tensile Stress(max) |
% |
-15 |
-15 |
-15 |
|
|
Change of Elongation(max) |
% |
-20 |
-20 |
-20 |
|
|
Compression Permanentset |
175°Cx70h |
% |
≤20 |
≤20 |
≤20 |
|
Color |
|
|
Brown |
Black |
Red |
|
Applications |
Temperature Limited |
℃ |
-20~+250 |
-20~+200 |
-20~+200 |
|
Pressure Limited |
Mpa |
0~35 |
|||
|
Working Environment |
|
Strong Caustics, moderate acids, chlorine, gases, water, steam, hydrocarbons, hydrogen and aluminum fluoride except element fluorine and fusion sodium. |
|||
Product detail pictures:

Related Product Guide:
Useful Tips For Installing The Teflon Envelope Gasket
What Is A PTFE Ring Gasket?
Fixed Competitive Price FEP Encapsulated O-Ring for Peru Factories, The product will supply to all over the world, such as: , , ,
Mabema AAI, Automated Ammunition Inspection, is an inline inspection machine developed for quality inspection of cases and cartridges. It inspects cases and cartridges at high rate. Four cameras provide a 100% surface inspection.
Measurement examples:
• Split cases
• Scratches
• Dents
• Wrinkles
• Case length
• Defective mouth
• Flange diameter, thickness and shape
• Wrong or missing head stamp
• Missing or misplaced primer
• Defective or missing extractor groove
• Mixed types