Best Price for Aflas O-Ring Wholesale to Montreal

Short Description:

Aflas based synthetic rubber, reinforced with carbon black and peroxide cured. Has good rapid gas decompression(FGD) resistant properties, which making it suitable for many high pressure gas applications. Temperature capability for this type compound is +5~+200℃. Technical Data Sheet Properties Units Typical value Hardness IRHD 84 Tensile strength MPa 22 Elongation at break % 189 Modulus at50% elongation MPa 4 Modulus at100% elongation MPa 12  


Product Detail

Product Tags

Related Video

Feedback (2)

, , ,
Best Price for Aflas O-Ring Wholesale to Montreal Detail:

Aflas based synthetic rubber, reinforced with carbon black and peroxide cured. Has good rapid gas decompression(FGD) resistant properties, which making it suitable for many high pressure gas applications. Temperature capability for this type compound is +5~+200℃.

Technical Data Sheet

Properties Units Typical value
Hardness IRHD 84
Tensile strength MPa 22
Elongation at break % 189
Modulus at50% elongation MPa 4
Modulus at100% elongation MPa 12

 


Product detail pictures:

Best Price for
 Aflas O-Ring Wholesale to Montreal detail pictures


Related Product Guide:
What Is A PTFE Ring Gasket?
A Look at the Molded Gasket

Best Price for Aflas O-Ring Wholesale to Montreal, The product will supply to all over the world, such as: , , ,


  • I built a physical deposition chamber, for now it’s just evaporative deposition but I plan on adding a few other variants. The thin films created can be used in many ways.
    The chamber still has a ton of space leftover and I have some more equipment coming so hopefully I can do more interesting things.
    Sorry there’s no footage of lathing the feedthroughs, they worked nice with a cut o-ring and some heat shrink. Make sure you cut a slot down the holding screw threads to vent behind em. The 2 copper feedthroughs allow (with a center tap) 2 tungsten boats with different metals so I can avoid opening the chamber in a multi layer coating.
    The pump down takes about 45 min. to get to 10e-5. I can use a small steel hemisphere with a kf40 hose on the top for use with a secondary high vacuum chamber. The shutter was aluminum flashing with some steel stuck on one side so a neodymium magnet on the outside of the bell jar could move it around without a feedthrough.
    This build was really fun

    I got everything from mcmaster, K.j lesker, ebay and what I already had

    This did cost a bit to make:
    diffusion pump- $160
    mechanical pump-$140
    plate- $270 (ouch!)
    valves- $90
    gauges- $200
    misc vacuum stuff -$120
    bell jar – $140 (stupid)
    other stuff – maybe $100?

    I recommend you check out https://www.youtube.com/user/bkraz333
    he has done some neat stuff with his setup and a bunch of other things